Nimonic 86 Alloy 86 Ni Cr Mo Superalloy Forgings for Gas Turbine Combustion Chambers Heat-Treat Furnaces Nimonic 86 Alloy 86 Ni Cr Mo Superalloy Forgings for Gas Turbine Combustion Chambers Heat-Treat Furnaces

Nimonic 86 Alloy 86 Ni Cr Mo Superalloy Forgings for Gas Turbine Combustion Chambers Heat-Treat Furnaces

1500.0 USD ($)/Piece

Product Details:

  • Surface Treatment Mill Finish
  • Hardness 160 - 220 HBW
  • Process Forging
  • Product Type Forged Products
  • Material Steel
  • Technology Forging
  • Application Machine Parts
  • Click to view more
X

Nimonic 86 Alloy 86 Ni Cr Mo Superalloy Forgings for Gas Turbine Combustion Chambers Heat-Treat Furnaces Price And Quantity

  • 1500.0 USD ($)/Piece
  • 1 Piece

Nimonic 86 Alloy 86 Ni Cr Mo Superalloy Forgings for Gas Turbine Combustion Chambers Heat-Treat Furnaces Product Specifications

  • Forging
  • Mill Finish
  • 160 - 220 HBW
  • Forged Products
  • Steel
  • Forging
  • Customized Millimeter (mm)
  • Machine Parts
  • Customized Kilograms (kg)

Nimonic 86 Alloy 86 Ni Cr Mo Superalloy Forgings for Gas Turbine Combustion Chambers Heat-Treat Furnaces Trade Information

  • Shanghai port Ningbo port
  • Telegraphic Transfer (T/T), Letter of Credit (L/C)
  • Within a certain price range free samples are available
  • Standard export seaworthy packing or customized according to customer requirements.
  • North America, South America, Middle East, Africa, Asia, Australia, Central America, Eastern Europe, Western Europe
  • All India
  • ISO 9001:2015, EN 10204 3.1 MTC

Product Description

Jiangsu Liangyi is an ISO 9001:2015-certified forging manufacturer in China supplying Nimonic 86 / Alloy 86 open-die forgings, seamless rolled rings and bars to gas-turbine, aerospace and industrial heat-treatment projects in India and worldwide. ("Nimonic" is a Special Metals trademark; Jiangsu Liangyi is independent.)

Why Nimonic 86 / Alloy 86 for Indian gas-turbine and furnace projects

Alloy 86 is a solid-solution Ni-Cr-Mo superalloy with magnesium and cerium micro-additions giving exceptionally good cyclic oxidation resistance at 1,050 C, high creep strength and good weldability. For India's gas-turbine, aerospace and heat-treatment sectors, Alloy 86 suits combustion-chamber liners, afterburner parts and furnace fixtures subject to repeated thermal cycling.

Documented capability

Gas turbines/aerospace: combustion-chamber liners, afterburner parts, transition ducts.

Industrial heat treatment: furnace fixtures and components.

General cyclic high-temperature: rings, discs, hubs, sleeves, shafts, bars.

Product range for Indian buyers

Forged bars, shafts; seamless rolled rings; combustion-chamber and afterburner-liner forgings; heat-treatment furnace fixtures; nozzles, discs, hubs, sleeves.

Material data

Chemistry (per Special Metals technical bulletin, wt%): Ni balance, Cr 25.0, Mo 10.0, C 0.05, Mg 0.015, Ce 0.03. Solution anneal 1,150 C + air cool; NOT age-hardenable; exceptionally good cyclic-oxidation resistance at 1,050 C. Same alloy across Nimonic 86 / Alloy 86.

Standards & quality

Manufactured to material standards commonly applied to this alloy family (ASTM B435 / B564-type product forms); controlled Mg/Ce melting; 100% UT + PT; cyclic-oxidation and creep-rupture data on request; EN 10204-3.1 / 3.2.

Commercial & logistics

Lead time by project; FOB Shanghai / CIF to Nhava Sheva, Mundra, Chennai, Kandla, Visakhapatnam.

Enquire with Jiangsu Liangyi: sales@jnmtforgedparts.com +86-13585067993 Jiangyin, Jiangsu, China.

Jiangsu Liangyi is an independent manufacturer; designations indicate the material supplied. Nimonic is a registered trademark of Special Metals Corporation; Jiangsu Liangyi does not manufacture or sell Nimonic-branded products and is not affiliated.



Superior Alloy for Extreme Environments

Nimonic 86 Alloy stands out for its extraordinary resistance to heat and corrosion, making it an ideal choice for components exposed to high thermal and mechanical stresses. Its unique composition ensures lasting performance in gas turbines and heat-treating furnaces, supporting continuous operation and reliability.


Made-to-Order Forgings for Versatile Applications

Each Nimonic 86 Alloy forging is meticulously produced to meet specific project requirements. This customization allows for seamless integration in various machine parts, improving operational efficiency and equipment lifespan in the energy and manufacturing sectors.

FAQ's of Nimonic 86 Alloy 86 Ni Cr Mo Superalloy Forgings for Gas Turbine Combustion Chambers Heat-Treat Furnaces:


Q: How is Nimonic 86 Alloy beneficial for gas turbine combustion chambers?

A: Nimonic 86 Alloy is engineered to withstand the intense heat, corrosive gases, and mechanical stress experienced in gas turbine combustion chambers, ensuring long-term durability and minimized maintenance.

Q: What is the typical process used to manufacture these superalloy forgings?

A: The superalloy is shaped through precision forging, a process which improves strength and structural integrity by compressing the material into specific forms, followed by controlled heat treatment to achieve the desired hardness and performance.

Q: When should I consider using Nimonic 86 Alloy forgings for my equipment?

A: Nimonic 86 Alloy forgings are ideal when your machinery operates in environments with high temperatures, mechanical loads, or corrosive atmospheres, such as in gas turbines, industrial furnaces, and specialized heat-treat equipment.

Q: Where can these customized forgings be used besides gas turbines?

A: Beyond gas turbines, Nimonic 86 Alloy forgings are also suitable for use in heat-treat furnaces, other high-temperature industrial equipment, and any machine parts that require exceptional heat and corrosion resistance.

Q: What are the hardness and surface characteristics of these forgings?

A: These forgings achieve a hardness rating of 160-220 HBW, offering a strong balance between wear resistance and machinability. They are supplied with a mill finish, which ensures a smooth, reliable surface ready for integration.

Q: How are the dimensions and weight of the forgings customized?

A: Dimensions and weight are fully customizable to meet client specifications. The manufacturer tailors each forging according to the required length, width, height, and total weight as specified by the customer.

Tell us about your requirement
product

Price: