1.4606 X5NiCrTiMoVB25-15-2 Iron-Base PH Superalloy Forgings for Turbines, Nuclear Valves Discs, Rings, Bars Jiangsu Liangyi

595.0 USD ($)/Piece

Product Details:

  • Surface Treatment Mill Finish
  • Hardness 200 HBW
  • Process Hot Forging
  • Product Type Forged Products
  • Material Steel
  • Technology Forging
  • Application Machine Parts
  • Click to view more
X

1.4606 X5NiCrTiMoVB25-15-2 Iron-Base PH Superalloy Forgings for Turbines, Nuclear Valves Discs, Rings, Bars Jiangsu Liangyi Price And Quantity

  • 1 Piece
  • 595.0 USD ($)/Piece

1.4606 X5NiCrTiMoVB25-15-2 Iron-Base PH Superalloy Forgings for Turbines, Nuclear Valves Discs, Rings, Bars Jiangsu Liangyi Product Specifications

  • Machine Parts
  • Forged Products
  • 200 HBW
  • Mill Finish
  • Customized GSM (gm/2)
  • Steel
  • SILVER
  • Hot Forging
  • Forging
  • Customized Millimeter (mm)

1.4606 X5NiCrTiMoVB25-15-2 Iron-Base PH Superalloy Forgings for Turbines, Nuclear Valves Discs, Rings, Bars Jiangsu Liangyi Trade Information

  • Shanghai port Ningbo port
  • Telegraphic Transfer (T/T), Letter of Credit (L/C)
  • Within a certain price range free samples are available
  • Standard export seaworthy packing or customized according to customer requirements.
  • Asia, Central America, North America, South America, Middle East, Africa, Australia, Eastern Europe, Western Europe
  • All India
  • ISO 9001:2015, EN 10204 3.1 MTC

Product Description

Need a proven 1.4606 / X5NiCrTiMoVB25-15-2 (EN-designated iron-base PH superalloy) forging supplier for high-temperature, high-strength, non-magnetic parts? Jiangsu Liangyi forges this -strengthened alloy service to 704 C, non-magnetic, cryogenic-capable to EN 10088-3 / EN 10269 and AMS 5731 / 5732. ISO 9001:2015 certified, VIM+VAR melted, 50+ countries.

Power generation & gas turbines:

Turbine discs, spacers, compressor impellers, casing and high-strength ring forgings

Nuclear:

Nuclear-service forgings, reactor-internal and auxiliary high-strength non-magnetic components

Valves & high-temperature equipment:

Valve-part forgings, high-temperature structural parts, fasteners (EN 10269 bolting)

Oil & gas & general:

Downhole and high-temperature forgings, fastener stock, shafts, discs, hubs, sleeves, custom forgings

Why buyers choose Jiangsu Liangyi:

ISO 9001:2015 certified; manufactured to EN 10088-3 / EN 10269 / EN 10302, AMS 5731 / 5732 / 5737

VIM + VAR / ESR melting; solution treat 980 C + age 720 C/16 h; room/elevated-temp tensile on request

100% UT + PT; EN 10204-3.1 / 3.2; rings to 5 m; 30 kg30 t

Grade note: 1.4606 / X5NiCrTiMoVB25-15-2. Generic, no trademark. Fe 53, Ni 25, Cr 15, Ti 2.

Request a quote from Jiangsu Liangyi: sales@jnmtforgedparts.com +86-13585067993 Jiangyin, Jiangsu, China worldwide export.

Jiangsu Liangyi is an independent manufacturer supplying 1.4606 / X5NiCrTiMoVB25-15-2.

Tell us about your requirement
product

Price:

Quantity
Select Unit

  • 50
  • 100
  • 200
  • 250
  • 500
  • 1000+
Additional detail
Mobile number

Email

Other Products in 'Custom Forging Parts' category



Back to top