A286 UNS S66286 Iron Base PH Superalloy Forgings for Gas Turbines, Aerospace and Oil and Gas Discs, Impellers, Fasteners and Rings Jiangsu Liangyi

A286 UNS S66286 Iron Base PH Superalloy Forgings for Gas Turbines, Aerospace and Oil and Gas Discs, Impellers, Fasteners and Rings Jiangsu Liangyi

1080.0 USD ($)/Piece

Product Details:

  • Process Hot Forging, Solution Treatment, Precipitation Aging, CNC Machining
  • Surface Treatment Mill Finish
  • Hardness 248-341 HB (Solution Treated & Aged)
  • Product Type Forged Products
  • Material Steel
  • Technology Forging
  • Application Machine Parts
  • Click to view more
X

A286 UNS S66286 Iron Base PH Superalloy Forgings for Gas Turbines, Aerospace and Oil and Gas Discs, Impellers, Fasteners and Rings Jiangsu Liangyi Price And Quantity

  • 1080.0 USD ($)/Piece
  • 1 Piece

A286 UNS S66286 Iron Base PH Superalloy Forgings for Gas Turbines, Aerospace and Oil and Gas Discs, Impellers, Fasteners and Rings Jiangsu Liangyi Product Specifications

  • Forged Products
  • 248-341 HB (Solution Treated & Aged)
  • Forging
  • SILVER
  • CUSTOMIZED Kilograms (kg)
  • Mill Finish
  • Steel
  • Machine Parts
  • Hot Forging, Solution Treatment, Precipitation Aging, CNC Machining
  • CUSTOMIZED Millimeter (mm)

A286 UNS S66286 Iron Base PH Superalloy Forgings for Gas Turbines, Aerospace and Oil and Gas Discs, Impellers, Fasteners and Rings Jiangsu Liangyi Trade Information

  • SHANGHAI PORT NINGBO PORT
  • Telegraphic Transfer (T/T), Letter of Credit (L/C)
  • Within a certain price range free samples are available
  • Standard export seaworthy packing or customized according to customer requirements
  • Australia, Central America, North America, South America, Asia, Eastern Europe, Western Europe, Middle East, Africa
  • All India
  • ISO 9001:2015, EN 10204 3.1 MTC

Product Description

Jiangsu Liangyi is an ISO 9001:2015-certified forging manufacturer in China supplying A286 / UNS S66286 (iron-base PH superalloy) open-die forgings, seamless rolled rings and bars to gas-turbine, aerospace, power and oil & gas projects in India and worldwide, to AMS 5731/5732 and ASTM A453 Grade 660 / A638 Type 660.

Why A286 / UNS S66286 for Indian gas-turbine and aerospace projects

A286 is the highest-strength iron-base precipitation-hardening superalloy ( Ni(Ti,Al)), holding 900 MPa with useful strength and creep resistance to ~704 C, non-magnetic and cryogenic-capable to -196 C, at a fraction of nickel-base-superalloy cost. For India's gas-turbine, aerospace, power and oil & gas sectors, S66286 suits turbine discs, compressor impellers, retaining rings and fastener stock.

Documented capability

Aerospace/gas turbines: turbine discs/spacers, compressor impellers, casings, retaining rings, fastener stock.

Oil & gas: downhole tools, valve/fastener forgings.

Power/nuclear: steam/gas-turbine components, reactor internal forgings, high-strength rings.

Automotive/industrial: turbocharger wheels/shafts, exhaust high-temperature fasteners.

Product range for Indian buyers

Forged bars, shafts; seamless rolled rings; turbine discs and spacers; compressor impellers; valve and retaining-ring forgings; fastener and bolting stock; nozzles, discs, hubs, sleeves.

Material data

Chemistry (UNS S66286, wt%): Fe balance, Ni 24.027.0, Cr 13.516.0, Ti 1.92.35, Mo 1.01.5, V 0.100.50, Al 0.35, B 0.0030.010, C 0.08. Solution treat ~980 C + age ~720 C/16 h. Non-magnetic; 900 MPa tensile; to ~704 C. Same alloy across A286 / S66286 / 1.4980 / Alloy 660.

Standards & quality

Manufactured to AMS 5731/5732/5737, ASTM A453 Gr 660, A638 Type 660, B637; VIM + VAR / ESR melting; 100% UT + PT; room/elevated-temp tensile on request; EN 10204-3.1 / 3.2.

Commercial & logistics

Lead time by project; FOB Shanghai / CIF to Nhava Sheva, Mundra, Chennai, Kandla, Visakhapatnam.

Enquire with Jiangsu Liangyi: sales@jnmtforgedparts.com +86-13585067993 Jiangyin, Jiangsu, China.

Jiangsu Liangyi is an independent manufacturer; designations indicate the material supplied. "A-286" is a generic grade name, not a trademark.

Tell us about your requirement
product

Price:

Quantity
Select Unit

  • 50
  • 100
  • 200
  • 250
  • 500
  • 1000+
Additional detail
Mobile number

Email

Other Products in 'Custom Forging Parts' category



Back to top